Chery recalls 53,882 Tiggo 5x and Omoda cars in China over a rear-axle weld defect

Chery is calling back 53,882 Tiggo 5x and Omoda vehicles in China to check rear axles that could break free while driving, with free repairs beginning November 27.

Vehicles recalled in China
53,882
Omoda 5 SUVs recalled in Malaysia
8,878
Production window for affected cars
June 6, 2022 – December 31, 2023
Repairs begin
November 27, 2026

What Happened

China's vehicle safety regulator published the recall on Friday, covering 53,882 cars split between the Tiggo 5x line and the Omoda family. The filing carries the campaign code S2026M0146V and applies to vehicles built from June 6, 2022 through December 31, 2023. Work under the recall starts on November 27, 2026, three weeks after the notice went public.

Vehicles recalled in China

53,882

Tiggo 5x and Omoda models built between mid-2022 and the end of 2023.

The fault lies in how the rear axle was put together. Where the trailing arm meets its sleeve, the assembly process could leave the metal insufficiently fused, so the weld ends up weaker than the design calls for. Drive the car hard enough and that seam can crack and tear apart, freeing the arm from the axle. With the link gone, the driver no longer controls the rear wheels and the risk of a serious collision rises sharply.

How the recall unfolded
  1. June 6, 2022 – December 31, 2023

    Build window for the cars covered by the Chinese recall.

  2. October 6, 2026

    A 2023 Omoda 5 loses its rear axle while travelling on a Malaysian highway.

  3. Following the incident

    Malaysia's Road Transport Department suspends registrations of the model and Chery recalls 8,878 Omoda 5 SUVs there, prompting wider risk checks across its domestic and export ranges.

  4. November 6, 2026

    The State Administration for Market Regulation announces the Chinese recall of 53,882 vehicles.

  5. November 27, 2026

    Chery begins inspecting axles and replacing affected units at no charge.

The same defect, two markets
China
53,882 Tiggo 5x and Omoda vehicles
Malaysia
8,878 Omoda 5 SUVs
Extra step in Malaysia
Registrations of the model temporarily halted by the transport department

Owners will not be charged for any of it. Workshops in Chery's authorised service network will read the build-date marking stamped on each rear axle and, where the part came from the suspect batch, fit a fresh assembly. The inspection itself is free, and the replacement axle is supplied at no cost.

Previously from Chery Automobile Co., Ltd.

Chery's safety record drew scrutiny in late October 2026, when the Tiggo 2 was awarded zero stars in Latin NCAP crash testing. Inspectors recorded the footwell collapsing and an engine-compartment fire risk during frontal impact evaluations.

Background drawn from MotorClaw's earlier coverage of Chery Automobile Co., Ltd.'s official releases.

Why this matters

The campaign puts more than 53,000 Chinese owners of Tiggo 5x and Omoda cars in line for a no-charge fix on a part that holds the rear wheels in place. It also extends a safety problem Chery first confronted in Malaysia, where authorities stopped registrations of the Omoda 5 and 8,878 SUVs were recalled.

Terms in This Story

Trailing arm
A suspension link that ties a rear wheel hub to the car's body, letting the wheel travel up and down while holding it in position.
Rear axle
The structural assembly at the back of a car that carries the rear wheels and connects them to the suspension.
State Administration for Market Regulation (SAMR)
China's central regulator for product safety and market rules, which registers and publishes vehicle recalls.
Source: MotorClaw News Desk

A brief summary; details can be imperfect — always verify against the original source.

How useful was this article?

Feedback goes to the MotorClaw Desk and does not subscribe you to email. Privacy.